120 high-probability publications. We are testing a new system for linking publications to authors. You can help! If you notice any inaccuracies, please sign in and mark papers as correct or incorrect matches. If you identify any major omissions or other inaccuracies in the publication list, please let us know.

Year Citation  Score
2019 Peng W, Smiadak DM, Boehlert MG, Mather S, Williams JB, Morelli DT, Zevalkink A. Lattice hardening due to vacancy diffusion in (GeTe)mSb2Te3 alloys Journal of Applied Physics. 126: 055106. DOI: 10.1063/1.5108659  0.448
2018 Weller D, Kunkel G, Ochs A, Morelli D, Anderson M. Observation of n-type behavior in Fe-doped tetrahedrite at low temperature Materials Today Physics. 7: 1-6. DOI: 10.1016/J.Mtphys.2018.10.003  0.481
2018 Ponnambalam V, Morelli DT. A novel method to synthesize bulk super saturated solid solutions Ge1-xSnx (x≤5.0%) Journal of Alloys and Compounds. 740: 42-46. DOI: 10.1016/J.Jallcom.2017.12.351  0.358
2017 Wiendlocha B, Kim S, Lee Y, He B, Lehr G, Kanatzidis MG, Morelli DT, Heremans JP. Correction: Eu(2+)-Eu(3+) valence transition in double, Eu-, and Na-doped PbSe from transport, magnetic, and electronic structure studies. Physical Chemistry Chemical Physics : Pccp. PMID 28604874 DOI: 10.1039/c7cp90127e  0.754
2017 Wiendlocha B, Kim S, Lee Y, He B, Lehr G, Kanatzidis MG, Morelli DT, Heremans JP. Eu(2+)-Eu(3+) valence transition in double, Eu-, and Na-doped PbSe from transport, magnetic, and electronic structure studies. Physical Chemistry Chemical Physics : Pccp. PMID 28345722 DOI: 10.1039/C7Cp00358G  0.783
2017 Williams JB, Mather SP, Page A, Uher C, Morelli DT. Increasing the thermoelectric power factor of Ge17Sb2Te20 by adjusting the Ge/Sb ratio Journal of Applied Physics. 122: 045105. DOI: 10.1063/1.4995430  0.627
2017 Weller DP, Stevens DL, Kunkel GE, Ochs AM, Holder CF, Morelli DT, Anderson ME. Thermoelectric Performance of Tetrahedrite Synthesized by a Modified Polyol Process Chemistry of Materials. 29: 1656-1664. DOI: 10.1021/Acs.Chemmater.6B04950  0.306
2017 Weller DP, Morelli DT. Rapid synthesis of zinc and nickel co-doped tetrahedrite thermoelectrics by reactive spark plasma sintering and mechanical alloying Journal of Alloys and Compounds. 710: 794-799. DOI: 10.1016/J.Jallcom.2017.03.272  0.367
2017 Waldrop SL, Morelli DT. Effect of non-stoichiometry on the thermal and electrical properties of polycrystalline PtSb2 at low temperature Journal of Alloys and Compounds. 701: 23-26. DOI: 10.1016/J.Jallcom.2017.01.121  0.473
2017 Sun H, Lu X, Morelli DT. Detrimental effect of powder processing on the thermoelectric properties of CoSi Journal of Materials Science. 52: 8293-8299. DOI: 10.1007/S10853-017-1045-2  0.598
2017 Hui S, Gao W, Lu X, Panda A, Bailey TP, Page AA, Forrest SR, Morelli DT, Pan X, Pipe KP, Uher C. Engineering Temperature-Dependent Carrier Concentration in Bulk Composite Materials via Temperature-Dependent Fermi Level Offset Advanced Energy Materials. 8: 1701623. DOI: 10.1002/Aenm.201701623  0.669
2016 Lehr GJ, Waldrop SL, Carr WD, Morelli DT. Effect of chemical pressure manipulation on the valence and thermoelectric properties of the intermediate valence compound YbCu2-xNixGe2 Proceedings of Spie. 9821. DOI: 10.1117/12.2228757  0.801
2016 Li J, Zhu M, Abernathy DL, Ke X, Morelli DT, Lai W. First-principles studies of atomic dynamics in tetrahedrite thermoelectrics Apl Materials. 4. DOI: 10.1063/1.4959961  0.337
2016 Sun H, Lu X, Morelli DT. Isovalent substitutes play in different ways: Effects of isovalent substitution on the thermoelectric properties of CoSi0.98B0.02 Journal of Applied Physics. 120: 035107. DOI: 10.1063/1.4959209  0.627
2016 Lu X, Yao W, Wang G, Zhou X, Morelli D, Zhang Y, Chi H, Hui S, Uher C. Band structure engineering in highly degenerate tetrahedrites through isovalent doping Journal of Materials Chemistry A. 4: 17096-17103. DOI: 10.1039/C6Ta07015A  0.701
2016 Lu X, Morelli DT, Wang Y, Lai W, Xia Y, Ozolins V. Phase Stability, Crystal Structure, and Thermoelectric Properties of Cu12Sb4S13-xSex Solid Solutions Chemistry of Materials. 28: 1781-1786. DOI: 10.1021/Acs.Chemmater.5B04796  0.564
2016 Williams JB, Morelli DT. Using Ge Secondary Phases to Enhance the Power Factor and Figure of Merit of Ge17Sb2Te20 Journal of Electronic Materials. 1-10. DOI: 10.1007/S11664-016-4858-X  0.447
2016 Williams JB, Mather S, Morelli DT. Effects of Sn Substitution on Thermoelectric Properties of Ge4SbTe5 Journal of Electronic Materials. 45: 1077-1084. DOI: 10.1007/S11664-015-4221-7  0.481
2015 Beekman M, Morelli DT, Nolas GS. Better thermoelectrics through glass-like crystals. Nature Materials. 14: 1182-5. PMID 26585077 DOI: 10.1038/Nmat4461  0.335
2015 James DJ, Lu X, Morelli DT, Brock SL. Solvothermal Synthesis of Tetrahedrite: Speeding Up the Process of Thermoelectric Material Generation. Acs Applied Materials & Interfaces. 7: 23623-32. PMID 26478950 DOI: 10.1021/Acsami.5B07141  0.598
2015 Williams JB, Lara-Curzio E, Cakmak E, Watkins T, Morelli DT. Enhanced thermoelectric performance driven by high-temperature phase transition in the phase change material Ge4SbTe5 Journal of Materials Research. DOI: 10.1557/Jmr.2015.124  0.426
2015 Ponnambalam V, Morelli DT. Improved thermoelectric properties in heavily doped FeGa3 Journal of Applied Physics. 118: 245101. DOI: 10.1063/1.4938474  0.428
2015 Lehr GJ, Morelli DT. Interplay of chemical expansion, Yb valence, and low temperature thermoelectricity in the YbCu2Si2−xGex solid solution Journal of Applied Physics. 117: 135101. DOI: 10.1063/1.4916786  0.817
2015 James D, Lu X, Nguyen AC, Morelli D, Brock SL. Design of lead telluride based thermoelectric materials through incorporation of lead sulfide inclusions or ligand stripping of nanosized building block Journal of Physical Chemistry C. 119: 4635-4644. DOI: 10.1021/Jp5127046  0.582
2015 Lu X, Morelli DT, Xia Y, Ozolins V. Increasing the Thermoelectric Figure of Merit of Tetrahedrites by Co-Doping with Nickel and Zinc Chemistry of Materials. 27: 408-413. DOI: 10.1021/Cm502570B  0.57
2015 Carr WD, Morelli DT. Influence of doping and solid solution formation on the thermoelectric properties of chalcopyrite semiconductors Journal of Alloys and Compounds. 630: 277-281. DOI: 10.1016/J.Jallcom.2015.01.043  0.533
2015 Carr WD, Morelli DT. The Thermoelectric Properties and Solubility Limit of CuFeS2(1−x)Se2x Journal of Electronic Materials. 45: 1346-1350. DOI: 10.1007/S11664-015-4029-5  0.491
2015 Ponnambalam V, Morelli DT. Thermoelectric Investigation of the Pseudo Binary System PbTe–CoSe2 Journal of Electronic Materials. 44: 2089-2094. DOI: 10.1007/S11664-015-3665-0  0.472
2015 Lehr GJ, Morelli DT, Jin H, Heremans JP. YbCu2Si2–LaCu2Si2 Solid Solutions with Enhanced Thermoelectric Power Factors Journal of Electronic Materials. 44: 1663-1667. DOI: 10.1007/S11664-014-3509-3  0.809
2015 Lai W, Wang Y, Morelli DT, Lu X. Thermoelectrics: From Bonding Asymmetry to Anharmonic Rattling in Cu12Sb4S13Tetrahedrites: When Lone-Pair Electrons Are Not So Lonely (Adv. Funct. Mater. 24/2015) Advanced Functional Materials. 25: 3618-3618. DOI: 10.1002/Adfm.201570159  0.451
2015 Lai W, Wang Y, Morelli DT, Lu X. From bonding asymmetry to anharmonic rattling in Cu12Sb4S13 tetrahedrites: When lone-pair electrons are not so lonely Advanced Functional Materials. 25: 3648-3657. DOI: 10.1002/Adfm.201500766  0.503
2014 Sun H, Lu X, Chi H, Morelli DT, Uher C. Highly efficient (In₂Te₃)x(GeTe)(3-3x) thermoelectric materials: a substitute for TAGS. Physical Chemistry Chemical Physics : Pccp. 16: 15570-5. PMID 24953478 DOI: 10.1039/C4Cp01294A  0.76
2014 Lara-Curzio E, May AF, Delaire O, McGuire MA, Lu X, Liu CY, Case ED, Morelli DT. Low-temperature heat capacity and localized vibrational modes in natural and synthetic tetrahedrites Journal of Applied Physics. 115. DOI: 10.1063/1.4878676  0.586
2014 Zhang Y, Ozoliniņš V, Morelli D, Wolverton C. Prediction of new stable compounds and promising thermoelectrics in the cu-Sb-Se system Chemistry of Materials. 26: 3427-3435. DOI: 10.1021/Cm5006828  0.356
2014 Waldrop S, Morelli D. Low-Temperature Thermoelectric Properties of PtSb2−x Te x for Cryogenic Peltier Cooling Applications Journal of Electronic Materials. 44: 1562-1565. DOI: 10.1007/S11664-014-3480-Z  0.451
2013 Lu X, Morelli DT. Natural mineral tetrahedrite as a direct source of thermoelectric materials. Physical Chemistry Chemical Physics : Pccp. 15: 5762-6. PMID 23503421 DOI: 10.1039/C3Cp50920F  0.515
2013 Lu X, Morelli DT. Rapid synthesis of high-performance thermoelectric materials directly from natural mineral tetrahedrite Mrs Communications. 3: 129-133. DOI: 10.1557/Mrc.2013.26  0.51
2013 Lehr GJ, Morelli DT, Jin H, Heremans JP. Enhanced thermoelectric power factor in Yb1-xSc xAl2 alloys using chemical pressure tuning of the Yb valence Journal of Applied Physics. 114. DOI: 10.1063/1.4842795  0.794
2013 Ponnambalam V, Morelli DT, Bhattacharya S, Tritt TM. The role of simultaneous substitution of Cr and Ru on the thermoelectric properties of defect manganese silicides MnSiδ (1.73<δ<1.75) Journal of Alloys and Compounds. 580: 598-603. DOI: 10.1016/J.Jallcom.2013.07.136  0.425
2013 Schmidt RD, Case ED, Lehr GJ, Morelli DT. Room temperature mechanical properties of polycrystalline YbAl3, a promising low temperature thermoelectric material Intermetallics. 35: 15-24. DOI: 10.1016/J.Intermet.2012.11.019  0.786
2013 Lehr GJ, Morelli DT. Synthesis, crystal structure, and thermoelectric properties of the YbAl3-ScAl3 solid solution Intermetallics. 32: 225-229. DOI: 10.1016/J.Intermet.2012.08.014  0.802
2013 Lu X, Morelli D. The Effect of Te Substitution for Sb on Thermoelectric Properties of Tetrahedrite Journal of Electronic Materials. 43: 1983-1987. DOI: 10.1007/S11664-013-2931-2  0.65
2013 Ponnambalam V, Morelli DT. Thermoelectric Properties of Light-Element-Containing Zintl Compounds CaZn2−x Cu x P2 and CaMnZn1−x Cu x P2 (x = 0.0–0.2) Journal of Electronic Materials. 43: 1875-1880. DOI: 10.1007/S11664-013-2895-2  0.418
2013 Ponnambalam V, Morelli DT. On the Thermoelectric Properties of Zintl Compounds Mg3Bi2−x Pn x (Pn = P and Sb) Journal of Electronic Materials. 42: 1307-1312. DOI: 10.1007/S11664-012-2417-7  0.455
2013 Lehr GJ, Morelli DT. Thermoelectric Properties of Yb1−x (Er,Lu) x Al3 Solid Solutions Journal of Electronic Materials. 42: 1697-1701. DOI: 10.1007/S11664-012-2401-2  0.828
2013 Fan X, Case ED, Lu X, Morelli DT. Room temperature mechanical properties of natural-mineral-based thermoelectrics Journal of Materials Science. 48: 7540-7550. DOI: 10.1007/S10853-013-7569-1  0.576
2012 Zhang Y, Skoug E, Cain J, Ozoliņ V, Morelli D, Wolverton C. First-principles description of anomalously low lattice thermal conductivity in thermoelectric Cu-Sb-Se ternary semiconductors Physical Review B - Condensed Matter and Materials Physics. 85. DOI: 10.1103/Physrevb.85.054306  0.789
2012 Boona SR, Morelli DT. Relationship between structure, magnetism, and thermoelectricity in CePd3Mx alloys Journal of Applied Physics. 112: 063709. DOI: 10.1063/1.4754311  0.742
2012 Boona SR, Morelli DT. Enhanced thermoelectric properties of CePd3−xPtx Applied Physics Letters. 101: 101909. DOI: 10.1063/1.4751265  0.781
2012 Ganguly S, Zhou C, Morelli D, Sakamoto J, Brock SL. Synthesis and characterization of telluride aerogels: Effect of gelation on thermoelectric performance of Bi 2Te 3 and Bi 2-xSb xTe 3 nanostructures Journal of Physical Chemistry C. 116: 17431-17439. DOI: 10.1021/Jp3055608  0.564
2012 Boona SR, Morelli DT. Structural, Magnetic, and Thermoelectric Properties of Some CePd3-Based Compounds Journal of Electronic Materials. 42: 1592-1596. DOI: 10.1007/S11664-012-2328-7  0.799
2012 Sun H, Lu X, Morelli DT. Effects of Ni, Pd, and Pt Substitutions on Thermoelectric Properties of CoSi Alloys Journal of Electronic Materials. 42: 1352-1357. DOI: 10.1007/S11664-012-2211-6  0.562
2012 Yang H, Morelli DT. Improved Thermoelectric Properties in Ga2Te3-GaSb Vacancy Compounds Journal of Electronic Materials. 41: 1720-1724. DOI: 10.1007/S11664-012-2052-3  0.369
2012 Liu C, Morelli DT. Low-Temperature Thermoelectric Properties of Fe2VAl with Partial Cobalt Doping Journal of Electronic Materials. 41: 1632-1635. DOI: 10.1007/S11664-012-2025-6  0.502
2012 Skoug EJ, Cain JD, Morelli DT. Improved thermoelectric performance in cu-based ternary chalcogenides using S for Se substitution Journal of Electronic Materials. 41: 1232-1236. DOI: 10.1007/S11664-012-1969-X  0.799
2012 Zhang L, Zhou C, Morelli D, Sakamoto J. Scavenging Elemental Sb Through Addition of NbSb2 to Mm0.9Fe3.5Co0.5Sb12 Skutterudites Journal of Electronic Materials. 41: 1601-1605. DOI: 10.1007/S11664-011-1893-5  0.503
2012 Majsztrik PW, Kirkham M, Garcia-Negron V, Lara-Curzio E, Skoug EJ, Morelli DT. Effect of thermal processing on the microstructure and composition of Cu-Sb-Se compounds Journal of Materials Science. 1-11. DOI: 10.1007/S10853-012-6994-X  0.762
2012 Lu X, Morelli DT, Xia Y, Zhou F, Ozolins V, Chi H, Zhou X, Uher C. High Performance Thermoelectricity in Earth-Abundant Compounds Based on Natural Mineral Tetrahedrites Advanced Energy Materials. 3: 342-348. DOI: 10.1002/Aenm.201200650  0.733
2011 Skoug EJ, Morelli DT. Role of lone-pair electrons in producing minimum thermal conductivity in nitrogen-group chalcogenide compounds. Physical Review Letters. 107: 235901. PMID 22182103 DOI: 10.1103/Physrevlett.107.235901  0.782
2011 Skoug EJ, Cain JD, Morelli DT. Thermoelectric properties of Ge-doped Cu 3SbSe 4 Materials Research Society Symposium Proceedings. 1314: 1-6. DOI: 10.1557/Opl.2011.266  0.759
2011 Kirkham M, Majsztrik P, Skoug E, Morelli D, Wang H, Porter WD, Payzant EA, Lara-Curzio E. High-temperature order/disorder transition in the thermoelectric Cu 3SbSe3 Journal of Materials Research. 26: 2001-2005. DOI: 10.1557/Jmr.2011.43  0.801
2011 Ponnambalam V, Lehr G, Morelli DT. Influence of p- and n-type doping on the transport properties of the Nowotny chimney-ladder compounds RuAl2 and RuGa2 Journal of Materials Research. 26: 1907-1912. DOI: 10.1557/Jmr.2011.126  0.772
2011 Skoug EJ, Cain JD, Majsztrik P, Kirkham M, Lara-Curzio E, Morelli DT. Doping effects on the thermoelectric properties of Cu3SbSe4 Science of Advanced Materials. 3: 602-606. DOI: 10.1166/Sam.2011.1189  0.799
2011 Skoug EJ, Cain JD, Morelli DT, Kirkham M, Majsztrik P, Lara-Curzio E. Lattice thermal conductivity of the Cu3SbSe4-Cu 3SbS4 solid solution Journal of Applied Physics. 110. DOI: 10.1063/1.3610385  0.798
2011 Skoug EJ, Cain JD, Morelli DT. High thermoelectric figure of merit in the Cu3SbSe4-Cu3SbS4solid solution Applied Physics Letters. 98: 261911. DOI: 10.1063/1.3605246  0.729
2011 Zhou C, Sakamoto J, Morelli D, Zhou X, Wang G, Uher C. Thermoelectric properties of Co0.9Fe0.1Sb3-based skutterudite nanocomposites with FeSb2nanoinclusions Journal of Applied Physics. 109: 063722. DOI: 10.1063/1.3554403  0.615
2011 Ganguly S, Zhou C, Morelli D, Sakamoto J, Uher C, Brock SL. Synthesis and evaluation of lead telluride/bismuth antimony telluride nanocomposites for thermoelectric applications Journal of Solid State Chemistry. 184: 3195-3201. DOI: 10.1016/J.Jssc.2011.09.031  0.666
2011 Zhou C, Morelli D, Zhou X, Wang G, Uher C. Thermoelectric properties of P-type Yb-filled skutterudite Yb xFeyCo4-ySb12 Intermetallics. 19: 1390-1393. DOI: 10.1016/J.Intermet.2011.04.015  0.615
2011 Lu X, Morelli DT. Thermoelectric Properties of Mn-Doped Cu2SnSe3 Journal of Electronic Materials. 41: 1554-1558. DOI: 10.1007/S11664-011-1873-9  0.616
2011 Ponnambalam V, Morelli DT. Effect of Cr and Fe Substitution on the Transport Properties of the Nowotny Chimney–Ladder MnSi δ (1.73 < δ < 1.75) Compounds Journal of Electronic Materials. 41: 1389-1394. DOI: 10.1007/S11664-011-1843-2  0.358
2011 Zhou C, Sakamoto J, Morelli D. High-Temperature Thermoelectric Properties of p-Type Yb-Filled Skutterudite Nanocomposites with FeSb2 Nanoinclusions Journal of Electronic Materials. 41: 1030-1035. DOI: 10.1007/S11664-011-1831-6  0.553
2011 Boona SR, Morelli DT. Thermoelectric Properties of Ce1−x Sc x Pd3 Journal of Electronic Materials. 41: 1199-1204. DOI: 10.1007/S11664-011-1788-5  0.79
2011 Liu C, Morelli DT. Thermoelectric Properties of Hot-Pressed and PECS-Sintered Magnesium-Doped Copper Aluminum Oxide Journal of Electronic Materials. 40: 678-681. DOI: 10.1007/S11664-011-1508-1  0.511
2010 Skoug EJ, Cain JD, Morelli DT. Structural effects on the lattice thermal conductivity of ternary antimony- and bismuth-containing chalcogenide semiconductors Applied Physics Letters. 96: 181905. DOI: 10.1063/1.3425886  0.793
2010 Skoug EJ, Cain JD, Morelli DT. Thermoelectric properties of the Cu2SnSe3–Cu2GeSe3 solid solution Journal of Alloys and Compounds. 506: 18-21. DOI: 10.1016/J.Jallcom.2010.06.182  0.818
2010 Zhou C, Sakamoto J, Morelli D. Low-Temperature Thermoelectric Properties of Co0.9Fe0.1Sb3-Based Skutterudite Nanocomposites with FeSb2 Nanoinclusions Journal of Electronic Materials. 40: 547-550. DOI: 10.1007/S11664-010-1444-5  0.544
2009 Liu C, Ren F, Wang H, Case ED, Morelli DT. SOLID-STATE SYNTHESIS AND SOME PROPERTIES OF MAGNESIUM-DOPED COPPER ALUMINUM OXIDES Mrs Proceedings. 1218. DOI: 10.1557/Proc-1218-Z01-05  0.495
2009 Morelli DT, Skoug EJ. Ternary Copper-Based Diamond-Like Semiconductors for Thermoelectric Applications Mrs Proceedings. 1166. DOI: 10.1557/Proc-1166-N06-07  0.785
2009 Skoug E, Zhou C, Pei Y, Morelli DT. High thermoelectric power factor in alloys based on CoSi Applied Physics Letters. 94: 022115. DOI: 10.1063/1.3072799  0.791
2009 Skoug EJ, Zhou C, Pei Y, Morelli DT. High Thermoelectric Power Factor Near Room Temperature in Full-Heusler Alloys Journal of Electronic Materials. 38: 1221-1223. DOI: 10.1007/s11664-008-0626-x  0.764
2008 Morelli DT, Jovovic V, Heremans JP. Intrinsically minimal thermal conductivity in cubic I-V-VI2 semiconductors Physical Review Letters. 101. DOI: 10.1103/Physrevlett.101.035901  0.456
2007 Kong H, Shi X, Uher C, Morelli DT. Thermoelectric properties of rare earth-ruthenium-germanium compounds Journal of Applied Physics. 102. DOI: 10.1063/1.2753592  0.553
2003 Yang J, Morelli DT, Meisner GP, Chen W, Dyck JS, Uher C. Effect of Sn substituting for Sb on the low-temperature transport properties of ytterbium-filled skutterudites Physical Review B. 67. DOI: 10.1103/PhysRevB.67.165207  0.638
2002 Yang J, Morelli DT, Meisner GP, Chen W, Dyck JS, Uher C. Influence of electron-phonon interaction on the lattice thermal conductivity ofCo1−xNixSb3 Physical Review B. 65. DOI: 10.1103/PhysRevB.65.094115  0.604
2002 Morelli DT, Heremans JP. Thermal conductivity of germanium, silicon, and carbon nitrides Applied Physics Letters. 81: 5126-5128. DOI: 10.1063/1.1533840  0.309
2000 Yang J, Meisner GP, Morelli DT, Uher C. Iron valence in skutterudites: Transport and magnetic properties ofCo1−xFexSb3 Physical Review B. 63. DOI: 10.1103/PhysRevB.63.014410  0.547
1999 Nolas GS, Morelli DT, Tritt TM. Skutterudites: a phonon-glass-electron crystal approach to advanced thermoelectric energy conversion applications Annual Review of Materials Science. 29: 89-116. DOI: 10.1146/Annurev.Matsci.29.1.89  0.344
1999 Uher C, Yang J, Hu S, Morelli DT, Meisner GP. Transport properties of pure and dopedMNiSn (M=Zr, Hf) Physical Review B. 59: 8615-8621. DOI: 10.1103/PhysRevB.59.8615  0.411
1998 Meisner GP, Morelli DT, Hu S, Yang J, Uher C. Structure and Lattice Thermal Conductivity of Fractionally Filled Skutterudites: Solid Solutions of Fully Filled and Unfilled End Members Physical Review Letters. 80: 3551-3554. DOI: 10.1103/PhysRevLett.80.3551  0.609
1997 Uher C, Chen B, Hu S, Morelli D, Meisner G. Transport Properties of Partially-Filled CeyCo4Sb12 Mrs Proceedings. 478. DOI: 10.1557/PROC-478-315  0.518
1997 Morelli DT, Meisner GP, Chen B, Hu S, Uher C. Cerium filling and doping of cobalt triantimonide Physical Review B. 56: 7376-7383. DOI: 10.1103/PhysRevB.56.7376  0.421
1997 Chen B, Xu J, Uher C, Morelli DT, Meisner GP, Fleurial J, Caillat T, Borshchevsky A. Low-temperature transport properties of the filled skutteruditesCeFe4−xCoxSb12s Physical Review B. 55: 1476-1480. DOI: 10.1103/Physrevb.55.1476  0.658
1996 Chen B, Uher C, Morelli DT, Mantese JV, Mance AM, Micheli AL. Large magnetothermopower in La0.67Ca0.33MnO3 films. Physical Review. B, Condensed Matter. 53: 5094-5097. PMID 9984098 DOI: 10.1103/Physrevb.53.5094  0.595
1996 Nolas GS, Slack GA, Morelli DT, Tritt TM, Ehrlich AC. The effect of rare-earth filling on the lattice thermal conductivity of skutterudites Journal of Applied Physics. 79: 4002. DOI: 10.1063/1.361828  0.344
1995 Morelli DT, Caillat T, Fleurial J, Borshchevsky A, Vandersande J, Chen B, Uher C. Low-temperature transport properties of p-type CoSb3. Physical Review. B, Condensed Matter. 51: 9622-9628. PMID 9977625 DOI: 10.1103/Physrevb.51.9622  0.645
1994 Uher C, Morelli DT. Influence of neutron irradiation on the thermal conductivity of vapor-deposited diamond Journal of Applied Physics. 76: 1515-1517. DOI: 10.1063/1.357727  0.452
1993 Morelli DT, Perry TA, Vandersande JW, Uher C. Glasslike thermal transport in heavily irradiated diamond. Physical Review. B, Condensed Matter. 48: 3037-3041. PMID 10008722 DOI: 10.1103/Physrevb.48.3037  0.508
1993 Morelli DT, Uher C. Correlating optical absorption and thermal conductivity in diamond Applied Physics Letters. 63: 165-167. DOI: 10.1063/1.110387  0.478
1993 Morelli DT, Uher C, Robinson CJ. Transmission of phonons through grain boundaries in diamond films Applied Physics Letters. 62: 1085-1087. DOI: 10.1063/1.108802  0.425
1992 Morelli DT. Thermal conductivity of high temperature superconductor substrate materials: Lanthanum aluminate and neodymium aluminate Journal of Materials Research. 7: 2492-2494. DOI: 10.1557/JMR.1992.2492  0.304
1992 Morelli DT. Spin–disorder scattering in europium-doped indium antimonide thin films Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures. 10: 110. DOI: 10.1116/1.586308  0.343
1991 Morelli DT, Doll GL, Heremans J, Peacor SD, Uher C, Dresselhaus MS, Cassanho A, Gabbe DR, Jenssen HP. Thermal conductivity of single crystal lanthanum cuprates at very low temperature Solid State Communications. 77: 773-776. DOI: 10.1016/0038-1098(91)90573-E  0.741
1990 Partin D, Heremans J, Morelli D, Thrush C. The Role of Rare Earths in Narrow Energy Gap Semiconductors Mrs Proceedings. 216. DOI: 10.1557/Proc-216-527  0.308
1989 Morelli DT, Doll GL, Heremans JP, Jenssen HP, Cassanho A, Dresselhaus MS. Anisotropic Thermal Conductivity of Superconducting Lanthanum Cuprate Mrs Proceedings. 169. DOI: 10.1557/Proc-169-1101  0.451
1989 Morelli DT, Heremans J, Doll G, Picone PJ, Jenssen HP, Dresselhaus MS. Thermal properties of single-crystal La2CuO4- Physical Review B. 39: 804-807. DOI: 10.1103/Physrevb.39.804  0.45
1988 Morelli DT, Beetz CP, Perry TA. Thermal conductivity of synthetic diamond films Journal of Applied Physics. 64: 3063-3066. DOI: 10.1063/1.341571  0.315
1988 Morelli DT, Heremans J. Thermal conductivity of single‐crystal barium fluoride Journal of Applied Physics. 63: 573-574. DOI: 10.1063/1.340090  0.369
1987 Heremans J, Morelli DT. Thermal Conductivity of Substituted Perovskite Superconductors Mrs Proceedings. 99. DOI: 10.1557/Proc-99-761  0.315
1986 Morelli DT, Heremans J, Sakamoto M, Uher C. Anisotropic heat conduction in diacetylenes. Physical Review Letters. 57: 869-872. PMID 10034182 DOI: 10.1103/Physrevlett.57.869  0.49
1986 Uher C, Morelli DT. Electrical resistivity of single crystal arsenic at very low temperatures Journal of Physics F: Metal Physics. 16. DOI: 10.1088/0305-4608/16/6/002  0.492
1985 Morelli DT, Uher C. Thermal conductivity and thermopower of graphite at very low temperatures. Physical Review. B, Condensed Matter. 31: 6721-6725. PMID 9935554 DOI: 10.1103/Physrevb.31.6721  0.522
1985 Clarke R, Morelli D, Uher C, Homma H, Schuller IK. Electronic transport in Mo/Ni superlattices Superlattices and Microstructures. 1: 125-129. DOI: 10.1016/0749-6036(85)90106-5  0.462
1985 Uher C, Morelli DT. Thermal transport properties of SbCl5-graphite and of HOPG in the c-direction Synthetic Metals. 12: 91-96. DOI: 10.1016/0379-6779(85)90093-1  0.515
1984 Morelli DT, Uher C. T2 dependence of the in-plane resistivity of graphite at very low temperatures Physical Review B. 30: 1080-1082. DOI: 10.1103/Physrevb.30.1080  0.457
1983 Morelli DT, Uher C. Thermal conductivity of arsenic single crystals from 2 to 300 K Physical Review B. 28: 4242-4246. DOI: 10.1103/Physrevb.28.4242  0.495
1983 Morelli DT, Uher C. C-axis electrical resistivity of SbCl5-graphites Physical Review B. 27: 2477-2479. DOI: 10.1103/Physrevb.27.2477  0.466
1982 Uher C, Morelli D. C-Axis Resistivity of SbCl5-Graphite in Hopg and Single Crystal Forms Mrs Proceedings. 20. DOI: 10.1557/Proc-20-163  0.492
1982 Morelli DT, Uher C. Thermopower measurements on arsenic from 2 to 300 K Physical Review B. 26: 6349-6354. DOI: 10.1103/Physrevb.26.6349  0.445
1982 Clarke R, Elzinga M, Gray JN, Homma H, Morelli DT, Winokur MJ, Uher C. Commensurate-incommensurate transitions in SbCl5 intercalated graphites Physical Review B. 26: 5250-5253. DOI: 10.1103/Physrevb.26.5250  0.663
1982 Elzinga M, Morelli DT, Uher C. Thermal transport properties of SbCl5 graphite Physical Review B. 26: 3312-3319. DOI: 10.1103/Physrevb.26.3312  0.747